What if an acrylic bar returns an unexpectedly low flexural modulus? Before changing the cutter, match the specimen number on the load trace to the dimensions entered for that bar. The sheet label and the measured thickness are two different entries.

Use the single-flute AAA bit to profile the sides of a rectangular blank while leaving the two sheet faces intact. The 3.175×1.0×4 model has a 1 mm cutting diameter and 4 mm of cutting edge. Check the job against the usable reach of the mounted tool. Measure the finished width and thickness before sending the bar for testing.
Lay the bar flat across the two supports. The loading nose acts halfway between them. Measure the span between the two support contact lines. Exclude the overhang at either end. For a small-deflection, three-point test on a uniformly rectangular bar, the tangent flexural modulus is mL³/(4bd³). Here m is the initial linear slope of load versus midspan deflection, L the span, b the width and d the thickness.
Suppose the bar measured 2.80 mm but the file used 3.00 mm from the sheet label. Keep the same trace, width and span. The reported modulus is (2.80/3.00)³ times the corrected value, about 81%. Correct that input and retain the original trace. This recalculation alone cannot tell the shop whether milling changed the acrylic.